The spraying process provides dual protection and beautification for aluminum and magnesium alloy products. It significantly enhances appearance texture and visual appeal, while effectively improving corrosion resistance, wear resistance, high-temperature resistance, and UV resistance, extending service life and adapting to complex environments (outdoor exposure, high-temperature working conditions, acid-base corrosion, humidity, etc.).
We provide diversified and customized spraying solutions according to customer needs, application scenarios, and budgets, covering conventional and high-end special spraying. We offer liquid painting, electrostatic powder coating, PVD vacuum plating, micro-arc oxidation (MAO), anodizing, and other surface treatment processes to meet full-scenario demands from ordinary decoration to high-end protection.
Liquid Painting Process
Liquid painting is one of the core processes for surface protection and decoration of aluminum-magnesium alloy products. It atomizes liquid paint through professional equipment to adhere uniformly to the surface, forming a dense and uniform protective coating after curing, combining decoration and functionality for multi-field applications. We adopt an automatic painting line with high-precision spraying robots and a special paint system, optimizing process parameters for the oxidation-prone and soft characteristics of aluminum-magnesium alloys to ensure strong adhesion, excellent durability, and high appearance consistency.
- Technical Details: Pre-treatment follows a four-step standard process: degreasing-water washing-phosphating-anodizing. Degreasing uses alkaline degreaser (concentration 5%–8%, temperature 50–60 ℃, soaking 5–10 minutes) with ultrasonic cleaning to remove oil, fingerprints, and impurities. Phosphating forms a 0.5–1.5 μm zinc-based phosphating film to enhance coating adhesion. Anodizing forms an additional 5–20 μm dense oxide film for further corrosion resistance. Electrostatic spraying is adopted with spray gun voltage 60–80 kV, current 10–20 μA, paint atomization particle size 10–50 μm, ensuring uniform coating without dead corners. Coating thickness is adjustable at 20–100 μm with error ≤±5 μm.
- Special paint systems for aluminum-magnesium alloys: acrylic paint and polyurethane paint for general decoration with good gloss and weather resistance; fluorocarbon paint (fluorine content ≥70%) for outdoor use with 15–20 years of non-fading and non-peeling performance; epoxy paint for industrial wear resistance with hardness HRC 25–30. Curing uses a constant-temperature oven with precise parameters: acrylic/polyurethane paint 80–120 ℃ for 20–30 minutes; fluorocarbon paint 180–220 ℃ for 25–35 minutes; epoxy paint 120–150 ℃ for 30–40 minutes, temperature uniformity ±3 ℃, ensuring tight bonding without bubbles, sagging, or pinholes.
- Technical Advantages: Automatic operation reduces manual errors with coating uniformity >99.5%. Special pre-treatment ensures coating adhesion ≥1.5 MPa, not easy to peel. Diversified paint adapts to outdoor, high-temperature, and corrosive environments. No obvious color difference (ΔE ≤2.0), customizable colors, balancing decoration and protection.
Electrostatic Powder Coating Process
Electrostatic powder coating is an eco-friendly high-end surface treatment technology. It uses electrostatic adsorption to atomize and charge solvent-free solid powder, which adheres uniformly to the product surface and forms a dense, tough protective coating after high-temperature curing, combining environmental friendliness, wear resistance, and corrosion resistance for mass-produced industrial, outdoor, and decorative parts. We adopt a fully automatic electrostatic powder coating line with an intelligent powder recovery system, optimizing processes for aluminum-magnesium alloy substrates to balance efficiency and coating quality.
- Technical Details: Pre-treatment: degreasing-water washing-phosphating-drying. Neutral degreaser (concentration 3%–5%, temperature 45–55 ℃, soaking 3–8 minutes) with high-pressure spray cleaning removes oil and oxide scale. Zinc-based phosphating solution (35–45 ℃, 2–4 minutes) forms a 0.3–1.0 μm phosphating film. Hot-air circulation drying (80–100 ℃, 10–15 minutes) ensures surface moisture ≤0.1 mg/cm² to avoid bubbles. High-voltage electrostatic spray gun: voltage 60–90 kV, current 20–30 μA, distance 150–300 mm, powder particle size 20–80 μm. Coating thickness 50–120 μm with error ≤±5 μm, one-time qualification rate >95%.
- Eco-friendly powder coatings meeting RoHS: epoxy-polyester for indoor decoration; fluorocarbon powder for outdoor use with 30-year weather resistance; pure epoxy powder for industrial wear resistance with hardness HRC 30–35. Three-stage temperature-controlled curing (preheating 180 ℃, curing 200 ℃, cooling) for 15–25 minutes, temperature uniformity ±2 ℃. Cyclone separation + filter recovery system achieves powder recovery rate ≥95% and coating utilization >98%, reducing costs by 40% compared with traditional painting.
- Technical Advantages: Eco-friendly with no VOC emissions, recyclable powder. Dense coating (porosity <0.3%) with adhesion ≥0 grade. Neutral salt spray test ≥1000 hours. Matte, glossy, frosted, and orange-peel effects available, color difference ΔE ≤1.0. High automation efficiency.
PVD Vacuum Plating Process
PVD (Physical Vapor Deposition) vacuum plating is a high-end surface treatment technology. In a high-vacuum environment, metal or compound targets are converted into atoms, molecules, or ions via evaporation or sputtering, depositing on the product surface to form a dense, uniform coating with high-end decoration and excellent protection for high-end products. We adopt imported high-vacuum coating equipment, optimizing parameters for aluminum-magnesium alloys to achieve perfect bonding between coating and substrate.
- Technical Details: Pre-treatment: degreasing-water washing-polishing-ion cleaning. Polishing ensures surface roughness Ra ≤0.8 μm; argon ion bombardment removes oxide layer and impurities. Vacuum degree controlled at 1×10⁻³–1×10⁻⁵ Pa. High-purity targets (titanium, chromium, aluminum, gold, TiN, TiC, etc.) with purity ≥99.99%. Evaporation coating (1500–2000 ℃, deposition rate 0.1–0.5 μm/min, thickness 0.1–1.0 μm) for large-area high-gloss products; magnetron sputtering (power 500–1500 W, rate 0.05–0.2 μm/min, thickness 0.05–0.5 μm) for complex structures. Vacuum annealing (150–250 ℃, 30–60 minutes) relieves stress and improves hardness and adhesion.
- Technical Advantages: Dense coating (porosity <0.5%), neutral salt spray test ≥100 hours. High hardness (titanium coating HRC 60–70), excellent wear resistance. Conductive coating available. High-end metallic texture with matte, glossy, and brushed effects. Eco-friendly RoHS-compliant, ultra-thin coating (error ≤±0.01 μm) without affecting dimensional accuracy.
Micro-Arc Oxidation (MAO) Process
MAO, also known as micro-plasma oxidation, is a new surface treatment technology for light metals such as aluminum, magnesium, and titanium. High-voltage pulse electricity is applied in electrolyte to generate micro-arc discharge on the surface, forming a ceramic oxide film metallurgically bonded to the substrate via high-temperature and high-pressure reactions, providing superior corrosion, wear, and high-temperature resistance for high-end protection. We adopt customized MAO equipment, optimizing electrolyte and electrical parameters for aluminum-magnesium alloys to ensure stable and uniform oxide film.
- Technical Details: Pre-treatment: degreasing-water washing-degreasing-activation. Neutral degreaser avoids corrosion; dilute sulfuric acid (1%–2%) removes oxide layer. Alkaline silicate electrolyte (10–20 g/L, 30–50 ℃). Pulse voltage 300–600 V, frequency 50–100 Hz, duty cycle 10%–30%, oxidation time 15–60 minutes. Oxide film thickness 5–50 μm (error ≤±2 μm), adhesion ≥20 MPa. Hardness HV 500–1500, neutral salt spray test ≥200 hours, heat resistance 300–500 ℃.
- Technical Advantages: Eco-friendly with recyclable electrolyte. Integrated substrate and film for long-lasting protection. Adjustable thickness, color, and performance. High efficiency for mass production, fundamentally improving corrosion resistance.
Anodizing Process
Anodizing is a special surface treatment for aluminum-magnesium alloys. The product is used as an anode in electrolyte, and electrochemical oxidation forms a dense, uniform oxide film under DC or pulse voltage, solving the oxidation problem of aluminum-magnesium alloys.
- Technical Details: Pre-treatment: degreasing-water washing-alkaline washing-neutralization-activation. Alkaline degreaser (4%–6%, 40–50 ℃, 4–8 minutes); dilute NaOH (2%–3%) removes oxide scale; dilute HNO₃ (5%–8%) neutralizes alkali; dilute H₂SO₄ (1%–2%) activates the surface. Aluminum alloy uses sulfuric acid electrolyte (150–200 g/L, 18–22 ℃); magnesium alloy uses oxalic acid electrolyte (80–120 g/L, 25–30 ℃). DC voltage 12–20 V, current density 1–2 A/dm², oxidation time 20–60 minutes, forming 10–30 μm oxide film (porosity 5%–10%). Electrostatic sealing spraying with acrylic or polyurethane paint (15–40 μm particle size, 50–70 kV, 15–25 μA), curing at 100–130 ℃ for 25–35 minutes (temperature uniformity ±3 ℃).
- Technical Advantages: Strong adhesion (peel strength ≥15 MPa), neutral salt spray test ≥150 hours after sealing. Mature and efficient for mass production. Eco-friendly and non-toxic, fundamentally extending service life.